Density
|
1.42
|
g/cm³
|
ISO 1183
|
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg)
|
2.4
|
g/10 min
|
ISO 1133
|
Molding Shrinkage
|
|
|
ISO 294-4
|
Across Flow
|
1.9
|
%
|
|
Flow
|
2.0
|
%
|
|
Tensile Modulus
|
457000
|
psi
|
ISO 527-2
|
Tensile Stress (Yield)
|
10400
|
psi
|
ISO 527-2
|
Tensile Strain (Yield)
|
20
|
%
|
ISO 527-2
|
Nominal Tensile Strain at Break
|
40
|
%
|
ISO 527-2
|
Flexural Modulus
|
428000
|
psi
|
ISO 178
|
Charpy Notched Impact Strength
|
|
|
ISO 179/1eA
|
-40°F
|
4.8
|
ft·lb/in²
|
|
73°F
|
5.2
|
ft·lb/in²
|
|
Charpy Unnotched Impact Strength (73°F)
|
No Break
|
|
ISO 179/1eU
|
Heat Deflection Temperature
|
|
|
|
66 psi, Unannealed
|
329
|
°F
|
ISO 75-2/B
|
264 psi, Unannealed
|
208
|
°F
|
ISO 75-2/A
|
Melting Temperature 3
|
352
|
°F
|
ISO 11357-3
|
Flammability Classification
|
|
|
IEC 60695-11-10, -20
|
0.0315 in
|
HB
|
|
|
0.0591 in
|
HB
|
|
|
Melt Density
|
1.16
|
g/cm³
|
|
Specific Heat Capacity of Melt
|
0.717
|
Btu/lb/°F
|
|
|